RM新时代注册-首页

中空玻璃起霧,八成是第一道膠沒(méi)涂穩

時(shí)間:2026-10-26 來(lái)源:http://www.whooo.net/ 發(fā)布人:昌盛機械

很多門(mén)窗廠(chǎng)售后非常頭疼的,不是玻璃自爆,而是交工一兩年中空層開(kāi)始起霧。拆開(kāi)看,二道硅酮膠完好,問(wèn)題幾乎都出在緊貼鋁條的這一圈熱熔膠上——斷膠、縮膠、界面有氣線(xiàn),水汽就是從這些微縫鉆進(jìn)去的。

The biggest headache for many door and window factories' after-sales service is not glass self explosion, but the fogging of the hollow layer after one or two years of delivery. Upon opening, the second layer of silicone adhesive is intact, but almost all of the problems lie in the hot melt adhesive tightly attached to the aluminum strip - breakage, shrinkage, and air lines at the interface. Water vapor has penetrated through these micro cracks.

W.JT01丁基膠涂布機

這臺負責“第一道防線(xiàn)”的設備,核心就管三件事:溫度、壓力、速度。

This device, responsible for the 'first line of defense', focuses on three things: temperature, pressure, and speed.

膠缸一般控制在 110~140℃,膠嘴要比膠缸高5~10℃,溫度低了拉絲斷膠,高了膠條發(fā)軟塌邊。

The glue cylinder is generally controlled at 110-140 ℃, and the glue nozzle should be 5-10 ℃ higher than the glue cylinder. When the temperature is low, the wire drawing will break, and when the temperature is high, the glue strip will become soft and collapse.

液壓壓力決定出膠量,壓力波動(dòng)會(huì )讓膠條時(shí)粗時(shí)細;皮帶速度和壓輪動(dòng)作建議跟光電信號對齊,不然轉角處容易堆膠或露白。

Hydraulic pressure determines the amount of adhesive produced, and pressure fluctuations can cause the adhesive strip to become thicker and thinner; The belt speed and roller action must be aligned with the photoelectric signal, otherwise it is easy to accumulate glue or expose white at corners.

鋁條建議干凈無(wú)油,涂完30秒內合片,放太久表面結皮,后期會(huì )假粘脫落。

The aluminum strip must be clean and oil-free. Within 30 seconds after coating, it should be laminated. If left for too long, the surface will form a crust, which may cause false adhesion and detachment in the later stage.

現場(chǎng)調試記三個(gè)動(dòng)作就夠:

Three actions are sufficient for on-site debugging:

換鋁條規格先對中——鋁框中心、壓輪中心、雙膠嘴中心三線(xiàn)重合,不重合就會(huì )單邊不沾膠。

Align the specifications of the aluminum strip first - the center of the aluminum frame, the center of the pressure wheel, and the center of the double rubber nozzle overlap. If they do not overlap, one side will not stick to the adhesive.

首件必做破壞檢查:撕開(kāi)看斷面是否致密黑亮,有沒(méi)有氣泡和白線(xiàn),寬度全點(diǎn)≥7mm再批量跑。

The first piece must undergo a destructive inspection: tear open to see if the section is dense, black, and shiny, if there are bubbles and white lines, and if the width is ≥ 7mm at all points before running in bulk.

每班停機前熱態(tài)清嘴,用銅片刮嘴口(別用鐵器敲),超過(guò)4小時(shí)不開(kāi)機就把管路余膠頂干凈,否則第二天必堵頭。

Before stopping each shift, clean the nozzle in a hot state and scrape the nozzle with a copper sheet (do not use an iron tool to knock). If the machine is not turned on for more than 4 hours, clean the remaining rubber on the pipeline, otherwise it will be blocked the next day.

還有一個(gè)容易忽略的坑:冷膠狀態(tài)千萬(wàn)別推油缸退膠,固態(tài)膠會(huì )把活塞和膠缸拉傷,維修單就是這么來(lái)的。

There is another easily overlooked pitfall: do not push the oil cylinder to return the glue when it is in a cold state. Solid glue can strain the piston and rubber cylinder, and that's how the repair order comes about.

把“溫壓速調穩、首件撕檢、停機清膠”這三句釘在操作臺旁邊,起霧返修率通常能降一大半。

Nail the three sentences of "temperature pressure speed stabilization, first piece tearing inspection, and shutdown cleaning" next to the control panel, and the fog repair rate can usually be reduced by more than half.

聯(lián)系我們Contact us

  • 咨詢(xún)熱線(xiàn):0531-85717458 13705446998
  • 公司地址: 山東省德州市齊河安頭鄉企巢工業(yè)園
  • 掃碼聯(lián)系我們:

截屏,微信識別二維碼

微信號:13705446998

// RM新时代注册-首页
如何加入RM新时代 rm棋牌 RM新时代下载不了 RM新时代专业团队|首入球时间 新时代RM官方网站下载 RM新时代平台靠谱平台入口-百度知道 新时代RM|国际平台 新时代RM|国际平台 新时代手机平台官网 如何加入RM新时代